說道鑄鐵平臺檢測平臺退火,這是一個(gè)專業(yè)性和操作性比較強(qiáng)的實(shí)戰(zhàn)工作,光靠一張嘴來說是說不通說不穿的,今天就簡明扼要的講下關(guān)于鑄鐵平臺檢測平臺的退火種類,這里貴在普及,在這里我會盡量用一些通俗的話來講,以期達(dá)到能使入門者很快理解。
鑄鐵平臺檢測平臺退火有三種或四種類型
就拿汽車的發(fā)動機(jī)的飛輪來說,它是一個(gè)比較大型的鑄件,它的鑄造就需要完全退火或等溫退火,其目的是消除內(nèi)應(yīng)力,雜質(zhì)在鑄造的過程已經(jīng)燃燒掉,如果不消除內(nèi)部不對稱的應(yīng)力在高速運(yùn)轉(zhuǎn)的飛輪中有可能會撕裂,這樣是很危險(xiǎn)的。而退火的目的就是是鋼結(jié)構(gòu)由奧氏體變成珠光體。
在一些水果刀菜刀之類刀具上需要球化退火,也就是低溫退火,溫度的巨大變化容易導(dǎo)致鋼結(jié)構(gòu)脆性,也就是我們常說刀刃容易嘣豁口,而低溫退火完全可以彌補(bǔ)這一缺陷。一把好的刀具如果有合理的退火工藝它一般是不會崩壞的。
最后一種就是消除應(yīng)力退火。玩過電焊的都知道,焊條在焊接過程中溫度受熱不均勻這樣會是有殘余應(yīng)力,這時(shí)候需要放入小于300度的爐子里去除應(yīng)力,在此階段還要保持溫度,是殘余應(yīng)力一點(diǎn)點(diǎn)殆盡,這樣才會生產(chǎn)出合格的工件。
上面三條就是鑄造平臺的三種退火種類,這三種方法不同但是都有一個(gè)共同點(diǎn)就是為了改善鋼結(jié)構(gòu),消除內(nèi)應(yīng)力,減少鋼結(jié)構(gòu)內(nèi)部的雜質(zhì),使鋼產(chǎn)品達(dá)到優(yōu)秀的標(biāo)準(zhǔn)。
It is said that the cast iron platform inspection platform is annealed. This is a professional and operationally strong actual combat work. It can't be said that it can't be said by one mouth. Today, we will briefly explain the types of annealing on the cast iron platform inspection platform. Here, you are popular, here I will try to use some popular words, in order to achieve a quick understanding of the beginners.
Cast iron platform inspection platform annealing has three or four types
Take the flywheel of the engine of the car, it is a relatively large casting, its casting needs to be fully annealed or isothermally annealed, the purpose is to eliminate the internal stress, the impurities have been burned in the casting process, if not eliminated inside Symmetrical stresses can tear in high-speed flywheels, which is dangerous. The purpose of annealing is to change the steel structure from austenite to pearlite.
In some tools such as fruit knife kitchen knives, spheroidizing annealing is required, that is, low temperature annealing. The large temperature change easily leads to the brittleness of the steel structure. That is, we often say that the blade is easy to break the gap, and low temperature annealing can completely compensate for this defect. A good tool will generally not break if it has a reasonable annealing process.
The last one is stress relief annealing. Those who have played the electric welding know that the temperature of the welding rod is uneven during the welding process, so there will be residual stress. At this time, it is necessary to put the stress in the furnace less than 300 degrees to remove the stress. At this stage, the temperature is maintained, which is a little residual stress. Exhaustion, in order to produce qualified workpieces.
The above three are the three types of annealing of the casting platform. These three methods are different but have one thing in common in order to improve the steel structure, eliminate the internal stress, reduce the impurities inside the steel structure, and make the steel products reach excellent standards.
Company name: botou zhuoyuan mechanical equipment manufacturing co.,LTD
Registered
address: jiaohe development zone, botou city, hebei province
Fax
number: 0317-8031093
Contact
information: 15369812793 (WeChat with the same number) liansheng chu
Postcode:
062151
Enterprise
email:1358827475@qq.com
Account
Opening Bank: Botou Branch of Bank of China
Account
number: 100399943203
Agricultural
bank account number: 6228481739059615270
http://zhuoyuanjixie.com